Kodi wonongayo ingakwaniritse bwanji kukana kuvala komanso zofunikira pakukonza molondola kwambiri?

2026-05-11 0 Ndisiyireni uthenga

M'munda wa pulasitiki extrusion ndi jekeseni akamaumba, ndiscrew imodzindiye gawo lalikulu lamphamvu panjira yonse yopanga. Zopangidwa mwaluso komanso zopangidwa mwaluso, sizimangotsimikizira kukhazikika kwa zinthu zomwe zimatumizidwa komanso kupanga pulasitiki, komanso zimakhudzanso kulondola kwazinthu zomwe zamalizidwa komanso kupitilizabe kupanga. Poyang'anizana ndi zida zovuta zokhala ndi magalasi opangira magalasi, calcium carbonate, zodzaza mchere, ndi zowonjezera zowononga, kusunga kukana kwamphamvu komanso kusasunthika kosasunthika kwa gawo lofunikirali pansi pa katundu wanthawi yayitali, kukangana kwakukulu ndi kutentha kwakukulu kwakhala cholinga chaukadaulo kwa oyang'anira zida ndi akatswiri opanga ma process.

single-screw

Kuvala ndi Kuwonongeka: Zomwe Zimayambitsa Kutengera Zambiri Zopanga

Zinthu zomwe zimatsogolera ku kulephera kwa wononga kwanthawi yayitali zimagwirizana mwachindunji ndi zomwe zidakonzedwa. Zida zosiyanasiyana zimapanga njira zowonongeka zosiyanasiyana pa aSingle Screw,kufunafuna mayankho achitetezo omwe akutsata. Gome ili m'munsili likufotokoza mwachidule mitundu itatu ya kuwonongeka kwa zinthu ndi zotsatira zake:

Mtundu wa Zinthu / Mkhalidwe Main Zowonongeka Njira Kusintha Kwachindunji pa Single screw
Magalasi fiber, calcium carbonate, mineral fillers Abrasion ndi kudula ndi tinthu zolimba Mphepete za ndege za screw zimakhala zozungulira, kuwonetsa kuchepa kwachangu, chilolezo chikuwonjezeka
PVC, EVA, TPR ndi zida zina zotengera kutentha Mipweya yowononga (mwachitsanzo, HCl) yotulutsidwa pa kutentha kwakukulu Micro pores ndi kuponya pamwamba pazitsulo, kuwonongeka kwa mphamvu
High-viscosity kusungunuka kapena zinthu zobwezerezedwanso Kutentha kwapafupi chifukwa cha kupsyinjika kwakukulu kwa shear Kuthamanga kwapang'onopang'ono kutopa, ming'alu kapena spalling


Pakupanga kwenikweni, kuvala kwa abrasive ndi dzimbiri lamankhwala nthawi zambiri zimasinthana, zomwe zimakulitsa kuwonongeka kwa wononga. Chifukwa chake, chitetezo chokwanira chiyenera kupangidwa kuchokera kuzinthu zitatu: zakuthupi, zochizira kutentha, ndi umisiri wapamtunda.

Njira Zaukadaulo Zokulitsa Kukaniza Kuvala ndi Kulondola

Njira Zazikulu: Kutetezedwa Mwadongosolo kuchokera ku Chithandizo cha Base Material mpaka Kupaka Zolimba

Kuti akwaniritse kukana kwamphamvu komanso kulondola kwambiri, akatswiri opanga akatswiri amatengera njira zotsatirazi:

  • Base material kuzimitsa ndi kutentha- Gwiritsani ntchito chitsulo cha aloyi cha 38CrMoAlA, choziziritsira komanso kutentha kwambiri kuti mupeze mawonekedwe amtundu wa sorbite, chotsani kupsinjika ndikupereka kulimba kwapakati.
  • Mwatsatanetsatane akupera- Gwiritsani ntchito zopukutira zama cylindrical ndi CNC zolondola kwambiri kuti muwonetsetse kuti mbiri yaulendo wanu ikulondola. Kuwongoka, kulolerana kwa mamvekedwe a mawu, ndi kuuma kwa pamwamba aSingle Screwzimayendetsedwa pamlingo wa micron, kuchepetsa kusungunuka kwa mmbuyo ndi kukangana kwanuko.
  • Kuchuluka kwa nitriding- Pakani gasi kapena ayoni nitriding kupanga 0.3-0.6 mm woyera wosanjikiza pamwamba pa wononga, kukwaniritsa kuuma kwa HV900-1100, kumathandizira kwambiri kukana kuvala kwa abrasive ndikusunga kulimba kwapakati.
  • Electroplating kapena electroless plating- Pazinthu zowononga kwambiri (mwachitsanzo, PVC, fluoroplastics), onjezani chromium yolimba kapena nickel wosanjikiza pamwamba pa nitrided wosanjikiza kuti mutseke ma pores ndikuwonjezera kukana kwa dzimbiri, kwinaku muchepetse kusungunuka.
  • Kuwotcherera kwapawiri-aloyi (PTA kapena laser cladding)- Pazinthu zonyezimira kwambiri monga ulusi wagalasi, calcium carbonate, kapena zinthu zobwezerezedwanso, gwiritsani ntchito nickel-based kapena cobalt-based alloy pamalangizo othawirako, kukwaniritsa kuuma kuposa HRC60. Kapangidwe kaphatikizidwe kameneka kamalola wononga kuti ikhalebe yokhazikika ya pulasitiki komanso kuloledwa bwino pansi paziwongolero zothamanga kwambiri komanso malo owononga.

Precision Machining ndi Kufananitsa Njira: Kuwonetsetsa kuti Pulasitiki Yofanana ndi Kufanana Kwazinthu

Kulondola kwakukulu sikungokhudza kulolerana kwa zomangira zake zokha, komanso kuwongolera chilolezo pakati pa phula lakunja lakunja ndi khoma lamkati la mbiya. Zochitika zikuwonetsa kuti kuwongolera chilolezo pakati pa aSingle Screw ndi mbiya mkati mwa 0.10-0.20 mm (malingana ndi m'mimba mwake) imachepetsa kwambiri kusungunuka kwachitsulo ndikuwonjezera kutulutsa kwapadera. Kuphatikiza apo, magawo okhathamiritsa a geometric (chiŵerengero cha kupsinjika, chiŵerengero cha L/D) chofanana ndi mbiya zodyetsera mbiya zimatha kukwaniritsa kumeta ubweya wambiri pa liwiro lotsika, kuchepetsa kutentha kwa kutentha ndi pafupifupi 10 ° C, potero kumapangitsa kuti zinthu zikhale bwino komanso kuti zikhale zokhazikika.

Mayankho Onse Pazinthu Zovuta Zogwirira Ntchito

Pazinthu zapadera monga wood-plastic composite (WPC), mapulasitiki odzaza kwambiri ndi uinjiniya, ndi zida zobwezerezedwanso, opanga otsogola asintha kuchoka pagawo losavuta kupita ku ntchito zaukadaulo zophatikizika zomwe zimakhudza "kusankha zinthu - kapangidwe kazinthu - chithandizo chamtsogolo".

Mwachitsanzo, pa nayiloni yolimbitsidwa yokhala ndi ulusi wamagalasi wopitilira 30%, zomangira zimatha kupangidwa mosinthasintha komanso kuzama kwa tchanelo, ndikusintha kozungulira pamizu yowulukira kuti muchepetse kupsinjika. Kuphatikizidwa ndi kuwotcherera kwapawiri-aloyi kutsitsi ndi kupukuta pagalasi (kuuma kwapamtunda Ra ≤ 0.05 μm), izi zimachepetsa chiwopsezo cha depositi ya kaboni ndikuthandizira kuyeretsa.

single-screw

Kutsiliza: Kufunika Kwa Nthawi Yaitali Poikapo Ndalama Pantchito Yapamwamba

Mwachidule, aSingle Screwopangidwa ndi mapangidwe olondola komanso machiritso oteteza kangapo sikuti amangowonjezera moyo wake wautumiki, komanso amathandizira kutulutsa mphamvu ndi jekeseni, amachepetsa kukonzanso pafupipafupi, ndikuwonetsetsa kusasinthika kwazinthu. Pamene pulasitiki processing makampani kusankha wopanga ngatiMalingaliro a kampani Malingaliro a kampani Zhoushan Nanhaiya Plastic Machinery Co., Ltd.- omwe ali ndi unyolo wathunthu, zida zopangira makina olondola, komanso luso lambiri lamakampani - amapeza chitsimikizo chaukadaulo chokhazikika kuchokera ku screw, kutenthetsa mpaka zokutira pamwamba, kuyala maziko olimba a nthawi yayitali yokhazikika.